The "Jominy test” is used to find
Correct answer
(B) hardenability
Solution
The Jominy end-quench test is a standard method used in metallurgy to determine the hardenability of steels. Hardenability refers to the ability of a steel to form martensite when quenched, which is a measure of how deep a steel can be hardened.Let's evaluate the options:
(A) Young's modulus is a measure of the stiffness or elastic modulus of a material, typically determined by tensile tests.
(B) Hardenability is the correct property determined by the Jominy test.
(C) Yield strength is the stress at which a material begins to deform plastically, also typically determined by tensile tests.
(D) Thermal conductivity is a measure of a material's ability to conduct heat, determined by specific heat transfer experiments.Therefore, the Jominy test is specifically designed to measure hardenability.The final answer is
(A) Young's modulus is a measure of the stiffness or elastic modulus of a material, typically determined by tensile tests.
(B) Hardenability is the correct property determined by the Jominy test.
(C) Yield strength is the stress at which a material begins to deform plastically, also typically determined by tensile tests.
(D) Thermal conductivity is a measure of a material's ability to conduct heat, determined by specific heat transfer experiments.Therefore, the Jominy test is specifically designed to measure hardenability.The final answer is
Continue learning with Success Tracker
A step still unclear? Work through it with support
Use Success Tracker to ask about the reasoning, then try another GATE ME question to check your understanding.
AI-powered practice· Unlimited practice on eligible plans
- PYQs with solutions
- Attempt available previous-year questions, then compare your reasoning with the worked solution. Coverage varies by stream.
- Practice that adapts
- Choose a topic, work on weaker areas and bookmark questions to revisit. Your attempts feed your progress tracking.
- AI doubt support
- Ask follow-up questions about a step or concept while practising, instead of stopping at the final answer.
Unlimited practice is available on eligible plans. Free practice and AI usage have limits; check the current plan allowances before choosing.
This page stays readable without an account. AI responses can be wrong; check them against the solution and source material.
More questions on Heat Treatment
2026 Set 1 Q62A metal has FCC crystal structure with 2.71 g/cm of density and 26.98 g/mol of atomic weight.…2025 Set 1 Q20Among the following surface hardening processes, steel is heated to the lowest temperature in2024 Set 1 Q28The phases present in pearlite are2023 Set 1 Q51The atomic radius of a hypothetical face-centered cubic (FCC) metal is nm. The…2023 Set 1 Q52A steel sample with 1.5 wt.% carbon (no other alloying elements present) is slowly cooled from 1100…